Tribocorrosion of stellite 6 in sulphuric acid medium: electrochemical behaviour and wear

Abstract : Tribocorrosion of stellite 6 in sulphuric acid was studied with a pin-on-disc tribometer through test conditions of intermittent friction. The occurrence of a mechanism involving mechanical depassivation during friction and further repassivation during the latency period between two successive friction steps was demonstrated. Polarization curves measurements and wear measurements by weight loss together with microtopography surveys of the wear track allowed to determine the relation giving the evolution of the wear with the duration of the latency period, and the kinetic law ruling the electrochemical repassivation mechanism.
Type de document :
Article dans une revue
Wearables Business, Prism Business Media, 2004, 256 (9-10), pp.948-953. 〈10.1016/j.wear.2003.06.003〉
Domaine :
Liste complète des métadonnées

https://hal-centralesupelec.archives-ouvertes.fr/hal-01251137
Contributeur : Catherine Kruch <>
Soumis le : mardi 5 janvier 2016 - 16:35:12
Dernière modification le : jeudi 5 avril 2018 - 12:30:10

Identifiants

Collections

Citation

L Benea, P Ponthiaux, F Wenger, J Galland, D Hertz, et al.. Tribocorrosion of stellite 6 in sulphuric acid medium: electrochemical behaviour and wear. Wearables Business, Prism Business Media, 2004, 256 (9-10), pp.948-953. 〈10.1016/j.wear.2003.06.003〉. 〈hal-01251137〉

Partager

Métriques

Consultations de la notice

89